35jacob35
Petroleum
- Apr 11, 2019
- 5
I apply stl6 HFO with PTa on f6a material.
After machining the weld surface, there is no problem. weld surface checked with UT and liquid penetrant method
but after 3-4 days the all weld disbond from surface or seen big cracks.
do you have any suggest.
After machining the weld surface, there is no problem. weld surface checked with UT and liquid penetrant method
but after 3-4 days the all weld disbond from surface or seen big cracks.
do you have any suggest.