dear friend
i am nandita from India.
i would like to know the desposal of wood ash. we are using wood as fuel in Hot air genrator. the analysis result of wood ash is as under
ph 7.9
water soluble 2.739
ca 0.256
mg 0.005
Na 0.492
HCo3 1.635
cl 0.063
So4 0.288
SO3 0.240
Na2so4 0.426
water insoluble 97.261
Acid soluble 61.6
Cao 37.9
Mgo 3.6
Fe2o3 6.00
Al2o3 37.5
SIO2 7.3
SO3 7.3
Acid insoluble 37.5
organic matter 0.9
Moisture 1.36
all parameters are expressed in percentage on dry weight basis except PH and Moisture.
Moistere expressed in percentage by weight
PH measured on 10% suspension of dry ash powder
the water soluble analysis carried out on 10% suspension of dry ash powder
the chemical analysis of acid soluble carried out in Hcl.
nandita dave
i am nandita from India.
i would like to know the desposal of wood ash. we are using wood as fuel in Hot air genrator. the analysis result of wood ash is as under
ph 7.9
water soluble 2.739
ca 0.256
mg 0.005
Na 0.492
HCo3 1.635
cl 0.063
So4 0.288
SO3 0.240
Na2so4 0.426
water insoluble 97.261
Acid soluble 61.6
Cao 37.9
Mgo 3.6
Fe2o3 6.00
Al2o3 37.5
SIO2 7.3
SO3 7.3
Acid insoluble 37.5
organic matter 0.9
Moisture 1.36
all parameters are expressed in percentage on dry weight basis except PH and Moisture.
Moistere expressed in percentage by weight
PH measured on 10% suspension of dry ash powder
the water soluble analysis carried out on 10% suspension of dry ash powder
the chemical analysis of acid soluble carried out in Hcl.
nandita dave