weldgal

Industrial
Apr 28, 2006
46
Looking for recommendations on filler metal for welding 317L stainless to SA516-70 for a 650 deg F application. Typically use 309 for carbon to stainless joints, but would like to make sure that this particular dissimilar joint doesn't pose any additional issues.
 