Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations IDS on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Distance between welds 1

Status
Not open for further replies.

mazxx

Materials
Mar 15, 2005
5
If we use the ASME CODE, WHAT IS THE DISTANCE BETWEEN WELDS ? FOR PIPING
 
Replies continue below

Recommended for you

mazxx;
For piping, there is no recommended minimum distance between welds. Using good design practice I would offer this for your consideration regarding minimum distance between butt welds; 2*D for piping and 3*D for tubing. The rationale for the above recommendations is to avoid the effects of residual stress and the combined effects of the weld heat affected zones on each weld joint if they were adjacent to one another.
 
The spacing should be based of pipe wall thickness (t) not diameter.

To say the welds on say a 900mm pipe should 1800m part is a bit much.

In other forums I have see the spacing as 2t to 4t.
 
Status