Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations cowski on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Do ASME B16.5 flange ratings include NEMA SM23 swings? 3

Status
Not open for further replies.

btuchaser

Mechanical
May 11, 2006
1
NEMA SM23 allows variations in steam pressure and temperature to exceed maximums by 20% pressure and 50 deg F. Do the ASME B16.5 ratings include these swings or are the B16.5 values absolute maximums? For A-217 GR WC9 (material group 1.10) Class 1500# at 950 F, the allowable pressure is 1885 psig. If the piping design requires 1750 psig @ 950 F is a 1500# flange acceptable or do you have to apply the NEMA variations? Applying the +50 F temperature variation would force a the design into a class 2500# flange as a 1500# flange at 1000 F has a rating of only 1305 psig.
 
Replies continue below

Recommended for you

NEMA SM23 is for steam turbines.
ASME B16.5 is for pipe flanges.

As long as your design pressure @ temperature falls below the ASME B16.5 class, that is it, as I interpret it.

Perhaps my mechanical colleagues can provide more information.

"Do not worry about your problems with mathematics, I assure you mine are far greater."
Albert Einstein
Have you read FAQ731-376 to make the best use of Eng-Tips Forums?
 
Your piping code, ASTM B31.3 or B31.1 defines the allowable short term conditions that exceed the design values.

NozzleTwister
Houston, Texas
 
If you are in Canada, CSA Z662.03


"Do not worry about your problems with mathematics, I assure you mine are far greater."
Albert Einstein
Have you read FAQ731-376 to make the best use of Eng-Tips Forums?
 
btu....

Nozzle is correct.....it is the piping code of record that defines maximum pressure/tempersture transients above design

Give him a star !!