Do the Hollo-Bolts connections require seal

Status
Not open for further replies.

BluRay999

Structural
Sep 3, 2014
3
Hello!

When bolting to the hollow section using Hollo-Bolts (bolt hole drilled in the wall of hollow section as shown on attached image) is it good practice to use mastics to seal joint to prevent uncontrolled corrosion inside of hollow section/home/javid/Desktop/Untitled.jpg?

Thank you for your answers.
 
Replies continue below

Recommended for you

Treat is like any HSS member; Either seal it or paint/coat the ID if used outdoors. The bolts are 'almost' self-sealing; the problem is the raw' tubesteel exposed to atmosphere.
 