For caustic environment containing H2S and meet the definition of sour as per NACE MR 0103, does require testing and qualification for ssc? N06040 is not listed in NACE MR 0103 section 14.
 
Replies continue below

Recommended for you

Check 14.1.1.2 against the base requirements for A494 N06040. Then review clause 11.

Steve Jones
Corrosion Management Consultant


All answers are personal opinions only and are in no way connected with any employer.
 
Thank you Dr. Jones.

N06040 does not meet the chemical composition requirements in clause 14.1.1.2 of NACE MR 0103, hence qualifications are required as per clause 11.
 