90
does anybody knows the kg/cm^2 that is usual on bearings of Renk or other manufacturers, and how to calculate the load of a shaft on the bearings, i´m asking for some kind of calcule formulas.... thanks from the far away Africa
 
Replies continue below

Recommended for you

Typical shell surface loads for RENK (or similar) sleeve bearings are 1-2 N/mm2 (actual values depend of course on speed, lubrication etc.), calculated as follows:
p=Fr/(DxB)
p - bearing surface load [N/mm2]
Fr - radial load on the bearing [N]
D - bearing shell bore / shaft journal diameter [mm]
B - bearing shell length (radial part) [mm]

Fr results from rotor weight, radial magnetic force and external loads (coupling weight, hydraulic forces (if any), etc.).
Ask RENK for catalogues - they contain bearing dimensions as well as useful graphs (eg. bearing temp. vs speed for different surface loads).
 