mrmalcolm
Marine/Ocean
- Jan 24, 2024
- 42
Do test piece for Welding Process Qualification testing need to be carried out by qualified welders? Is it allowed that test piece weled by unqualified welders? Thank you.
Follow along with the video below to see how to install our site as a web app on your home screen.
Note: This feature may not be available in some browsers.
Thank you for your reply. Would it be more appropriate to choose a moderately skilled welder( (with or without a welding qualification certificate) to weld the WPS test assembly?On two levels, it can hardly be otherwise: A welder cannot "be qualified" on a WPS test weld if that WPS itself is not yet qualified.
On the other hand, should YOU (your company) always chose your best welder (of those available) to make the certification welds for a new WPS?
Your "best welder" will find ways by his or her skills and hands-on knowledge to make a "bad WPS instructions and requirements" pass the strength and bend requirements. But a "common welder", one less experienced or one who represents your "average welder" will "test the procedure" better by revealing problems or restrictions or PWHT or inclusions or weld prep access problems.
Obviously, you do not want to "just grab the cheapest, least experienced guy from the line" to work on verification of a new WPS. An incompetent or poor welder will screw up a valid WPS just as easy as he or she can screw up a 50 year old procedure. But, in truth, you do write and approve every WPS to "verify that it will produce good welds" if used properly.