We have installed 3.3KV, 8 MW generator sets.Recentlt one testing contractor conducted Double Test (Tan delta) and confirms that the insulation detoriates and require retesting after six months.
What is the optimum Tan delta value for healthy generator stator winding?
How to compare Tandelta value with Polarisation Value?
Subra
What is the optimum Tan delta value for healthy generator stator winding?
How to compare Tandelta value with Polarisation Value?