Can anyone please tell me the Cement mortar layer thickness of a 20 inch class 250 DI pipe? Does this layer thickness change with the pipe size?

Thanks



 
Replies continue below

Recommended for you

From manufacturers I know it varies with the pipe size but the mortar layer is 3-6 mm thickness with DN 40 to DN 1200 pipes.
 
Thanks. All the information was very usefull.
 