Materials
Nov 9, 2010
169
All, I read that Boron over .002% will promote carbides in ductile iron. I have struggled online and I can't seem to find the scientific source of this number.
I want to understand the mechanism of carbide formation.

Any ideas?

Thanks
 
Replies continue below

Recommended for you

From literature it is known that Boron is a carbide stabilizer. It increases the undercooling during solidification,thereby promoting carbide formation instead of graphite.

You may find some answer to your question from the reference below. It has been many years and I need to refresh,perhaps you can find in papers published by J.F Wallace,it was published in Trans AFS.



_____________________________________
"The richer we have become materially, the poorer we have become morally and spiritually." Martin Luther King Jr
 
I just stumbled on one link,see if it helps:

"Elimination and Neutralization of Boron in Ductile Irons
by
R. L. Naro – ASI International, Ltd., Cleveland, Ohio
J. F. Wallace and Yulong Zhu – Case Western Reserve University, Cleveland, Ohio"



_____________________________________
"The richer we have become materially, the poorer we have become morally and spiritually." Martin Luther King Jr
 
Status
Not open for further replies.

Part and Inventory Search

Sponsor