Dear colleagues,
Could your help me evaluate/understand micro structure anomaly (please find attached)?
This is DSS weld cup microstructure (photo TV31, TV32) and SDS one (photo SDD_weld) . Welded joint is in solution annealing condition.
It seems sigma phase formation, but very coarse (magnification was 500x). I have etched it by NaOH 15 sec (for attached photo). Etching by NaOH during 2 sec have given the same result as well as etching by Beraha's (white "island" in blue ferrite).
Am I right? I observe structure like this in the first time (we examine DSS/SDS in different condition very often...)
What is reason of formation this microstructure?
Thank you in advance
Could your help me evaluate/understand micro structure anomaly (please find attached)?
This is DSS weld cup microstructure (photo TV31, TV32) and SDS one (photo SDD_weld) . Welded joint is in solution annealing condition.
It seems sigma phase formation, but very coarse (magnification was 500x). I have etched it by NaOH 15 sec (for attached photo). Etching by NaOH during 2 sec have given the same result as well as etching by Beraha's (white "island" in blue ferrite).
Am I right? I observe structure like this in the first time (we examine DSS/SDS in different condition very often...)
What is reason of formation this microstructure?
Thank you in advance