mrmalcolm
Marine/Ocean
- Jan 24, 2024
- 42
Post-weld heat treatment may result in a reduced strength of the welded joint(Including base metal, heat affected zone, and welding consumables ).
Even for some high-strength steels such as ASTM A517, the impact energy of welding consumables will decrease after post weld heat treatment.
What is the mechanism behind this? (1) Why does the strength of welded joints decrease? (2) Why does the impact energy of ASTM A517 welding consumables decrease?
thanks
Even for some high-strength steels such as ASTM A517, the impact energy of welding consumables will decrease after post weld heat treatment.
What is the mechanism behind this? (1) Why does the strength of welded joints decrease? (2) Why does the impact energy of ASTM A517 welding consumables decrease?
thanks