I'm caught up on a material for a latching configuration.
I've been hours on Matweb and the best I can come up with is a 304/L - 60% elongation @ yeild - Youngs @ 28000 ksi.
Am I on the right track.
I need a 1/4" deflection with as little as possible deformation. 1 cycle.[the configuration is much like a backpack clip]
Any input would be greatly appreciated.

Thank you,
Steve Scott
 
You are quite mistaken regarding 304L stainless steel - it has nothing near 60 % elongation at yield. The elastic strain at yield would be miniscule - something like 0.002 (i.e. 0.2 %).

If you need high elastic deflection without plastic deformation, you need a spring material. Spring temper stainless steel like 301 or 302 are good (but expensive). Maybe you can consider a carbon steel: music wire, hard drawn, Cr-V, Cr-Si, etc.

Regards,

Cory

Please see FAQ731-376 for tips on how to make the best use of Eng-Tips Fora.
 
Thank you,

I should learn to completely read what is presented to me, not just what is highlited. The datasheet I was reading from was "Crucible Steel 304L Chromium-Nickel Steel".
I just smacked myself in the side of the head, I had it coming.

Would you know, off hand, a material designation for the materials you suggested.

Steve
 
Here are a few:

ASTM A 288
ASTM A 277
ASTM A 679
ASTM A 229
ASTM A 230

Regards,

Cory

Please see FAQ731-376 for tips on how to make the best use of Eng-Tips Fora.
 
Cory,

Thank you so very much!!!
This has been an awakening for me to be more careful and review rather than rush.

Once again, THANKS!

Steve


 
Status
Not open for further replies.

Part and Inventory Search

Sponsor

Back
Top