Mchel80
Mechanical
- Oct 29, 2010
- 10
Hi All,
I have two 1.8"OD Tube with a Wall of 1.4mm made of 17-4PH 105K Yield and I will be electron welding them together to a depth of 1mm. The Axial load of the 1.4mm tube is approx 345K lbf. I need to determine the axial strength of the 1mm weld sections. I could take the weld as the wall thickness and determine the tube strength, but due to the fusion welding i am not sure if the weld area is going to provide the same yield strength. Can you provide a suggestion for determining the weld strength.
MChel80
I have two 1.8"OD Tube with a Wall of 1.4mm made of 17-4PH 105K Yield and I will be electron welding them together to a depth of 1mm. The Axial load of the 1.4mm tube is approx 345K lbf. I need to determine the axial strength of the 1mm weld sections. I could take the weld as the wall thickness and determine the tube strength, but due to the fusion welding i am not sure if the weld area is going to provide the same yield strength. Can you provide a suggestion for determining the weld strength.
MChel80