Hello,
I want to know the mechanical properties of P 355-N written in EN 10217-1.
Unfortunately,I haven't access to this standard here, if someone has this standard,it would be highly apprecited to let me know the mechanical properties or sending me the pdf format of EN 10217-1

Thanks in advance,
Pardiss
 
Replies continue below

Recommended for you

P355N:
Rm= 490-630 MPa
Re20= 355 MPa up to incl. 16 mm
345 MPa over 16mm up to 40 mm

EN10127-1 is a standard that expliains how the European material names are formed.
The mechaniacal prperties of P355N can be found in
EN 10028-3
 