Dec 14, 2003 #1 sykimm Coastal Nov 30, 2003 35 KR I'm about to design concrete structure in corrosive condition using expoxy coated rebar. Please help me to get the proper and relevant BS code and recommendation in relation with "Epoxy" coated rebar, e.g, bond strength, etc.
I'm about to design concrete structure in corrosive condition using expoxy coated rebar. Please help me to get the proper and relevant BS code and recommendation in relation with "Epoxy" coated rebar, e.g, bond strength, etc.
Feb 4, 2005 #2 ANEDIAN Civil/Environmental Jan 12, 2005 6 NL Please refer to BS 7295 and see how far that will lead you. Goodluck in your design Anji Upvote 0 Downvote