I am looking for the measure equipment for the melt blowing process parameters.
I am interested in the tooling which would allow to measure the air velocity and temperature.
The assumed maximum velocity of the air would be approximately 250m/s and the air maximum temperature is assumed to be approximately 230degC.
In order to measure the air velocity and temperature I would also need a transverse system.
I would like to ask very kindly for any advices what equipment would be the best option (possibly in regard to the lowest price).
I came across some companies that manufacture the alike equipment and I await the responses to my pricing inquiries.
The equipment which allows to measure low speed air flows (e.g. 30m/s) is relatively non-expensive but a more capable equipment (250m/s) seems to be very dear. Like this one:
Thank you.
I am looking for the measure equipment for the melt blowing process parameters.
I am interested in the tooling which would allow to measure the air velocity and temperature.
The assumed maximum velocity of the air would be approximately 250m/s and the air maximum temperature is assumed to be approximately 230degC.
In order to measure the air velocity and temperature I would also need a transverse system.
I would like to ask very kindly for any advices what equipment would be the best option (possibly in regard to the lowest price).
I came across some companies that manufacture the alike equipment and I await the responses to my pricing inquiries.
The equipment which allows to measure low speed air flows (e.g. 30m/s) is relatively non-expensive but a more capable equipment (250m/s) seems to be very dear. Like this one:
Thank you.