Equivalent diameter in tensile test

Status
Not open for further replies.

isoca

Materials
Mar 16, 2008
58
A client has sent us a specification to manufacture 316L tubes (12.7 mm OD) wich indicates the tensile test shall be carried out using a gauge length of 5D, where D is the equivalent diameter. My question is, what does it mean by "equivalent diameter"?
The specimen shall be tested in full cross section.
Thanks
 
Replies continue below

Recommended for you

Equivalent diameter usually refers to the flow area of a tube. For a circular tube, the equivalent diameter will be equal to the ID.
 
Thanks for the answer, but I have a question.
If the equivalent diameter is related to flow area (cross section?), where does it come from that it is equal to the ID? As far as I understand, the ASTM E8M indicates that the gauge length must be equal to 5D where D is the external diameter.
 
I think your customer used the wrong terminology and this should be clarified with the customer. Equivalent and external seem like easy enough words to swap if English isn't a first language.
 
In the US people use 2" or 4D (outside) for tube GL.
In Europe it is more common to use 5D.
I have seen both OD and mean D used in the GL calculation.
At the end of the day it doesn't matter.
Annealed 316L will be up over 50% elong however they measure it.
Strain rate matters more.

= = = = = = = = = = = = = = = = = = = =
P.E. Metallurgy, consulting work welcomed
 
WHAT 316L material-tube specification, WHAT strain hardness and WHAT wall thickness?

Is this a structural tube or a fluid-flow ['hydraulic' quality] tube?

Regards, Wil Taylor
o Trust - But Verify!
o For those who believe, no proof is required; for those who cannot believe, no proof is possible. [variation, Stuart Chase]
o Unfortunately, in science what You 'believe' is irrelevant. ["Orion", HBA forum]
o Only fools and charlatans know everything and understand everything." -Anton Chekhov
 
The tube is an ASTM A213. We have a lot of experience in manufacturing this type of tubes, however in this case the client requests that for the tensile test the elongation shall be taken using a gauge length equal to 5D where D is the equivalent diameter. What is not clear to me is the meaning of "equivalent diameter", that's all.
Thank you
 
The client doesn't know themselves.
I would use the OD.
And you need to also report the value with a 2" GL in order to comply with A213

= = = = = = = = = = = = = = = = = = = =
P.E. Metallurgy, consulting work welcomed
 
Theoretically, equivalent diameter = Squad (OD^2-ID^2)

Practically, you can use equivalent diameter = (OD+ID)/2. Or, simply use equivalent diameter = OD

Intrinsically, all probably donot matter much, as Ed pointed out, since 316 material would have a large elongation value (unless the deformation rate >95% during manufacturing).

The key is to clarify with the customer.
 
Ok thanks for the information. Obviously it is something that I asked the client, but sometimes the answers tend to come too late.
 