Hi

Can anyone tell me the modern equivalent of EN38 please.

In BS790 part 3 table 19 for say 216M36, in the size column it quotes letters P, Q and R. Do these relate to the tensile strength as suggested in table 29 or something totally different that I've missed.

Thanks in advance
 
Replies continue below

Recommended for you

Hi azzt -

There is no modern near equivalent to EN38 (taken from PD6474:1976 -Two way index of the designation system used in BS970:1955 and later revisions).

You will need therefore to determine what mechanical properties you require, then choose a suitable steel from BS970 Pt3 1991. You might need to agree this change with your client.

The designators P, Q, R do indeed relate to tensile strength given in Table 29.


Andy
 
Andy

Thanks for the info, sorry to be a pain but what is PD6474:1976, where would one get a copy of it?

Cheers

allan
 
azzt - if you can post some more details about what you are trying to make and where you are located then I suspect you will get a number of suggestions of potential alloys which could be used.
 