I have been picking up the skills in modelling using VCCT. However, I have been stuck with the following errors:
- ***ERROR: in keyword *ELASTIC, file "VCCT-Coupon-1.inp", line 1222: OdbError: Tabular data for at least one option or suboption has either blank or zero valued row(s).
- ***ERROR: MATERIAL OPTIONS USING DISTRIBUTIONS CAN ONLY HAVE A SINGLE DATA LINE.
- ***ERROR: ELEMENT 1 HAS NO ELASTIC PROPERTY REFERENCE
(This goes on for all shell elements)
I do believe they are related. I am not sure how to express this any further. Any tips? Perhaps someone is willing to step out and provide some assistance.
Thank you,
Ethan
I have been picking up the skills in modelling using VCCT. However, I have been stuck with the following errors:
- ***ERROR: in keyword *ELASTIC, file "VCCT-Coupon-1.inp", line 1222: OdbError: Tabular data for at least one option or suboption has either blank or zero valued row(s).
- ***ERROR: MATERIAL OPTIONS USING DISTRIBUTIONS CAN ONLY HAVE A SINGLE DATA LINE.
- ***ERROR: ELEMENT 1 HAS NO ELASTIC PROPERTY REFERENCE
(This goes on for all shell elements)
I do believe they are related. I am not sure how to express this any further. Any tips? Perhaps someone is willing to step out and provide some assistance.