EU 160 and EN10160

Status
Not open for further replies.

alimohd20009

Petroleum
Sep 7, 2009
5
Hi
EU 160 has been replaced with EN10160 and I would like to know what is equivalent class A,B,C in EU 160 with EN 10160?
please send me your good comments as soon as possible.
 
Replies continue below

Recommended for you

No class A, B or C in this standard, only S or E.
It's about ultrasonic testing of flat steel product of thicknes 6 mm and above (reflection method)

Regards from Barcelona
G. García
 