During fit up, my welders will grind and smooth the bevel surfaces and adjacent base material.
After which, we will notify the Client for Inspection and the time taken for them to inspect may varies. Sometime 1 day, 2 days or even 3 days.
So we will use a masking tape to cover the surface as it predominantly expose to external environment.
However I was thinking is there a better way than this? Do you guys have any suggestions other than masking tape in order to minimize re-work ?
What are your thoughts? Do let me know.
During fit up, my welders will grind and smooth the bevel surfaces and adjacent base material.
After which, we will notify the Client for Inspection and the time taken for them to inspect may varies. Sometime 1 day, 2 days or even 3 days.
So we will use a masking tape to cover the surface as it predominantly expose to external environment.
However I was thinking is there a better way than this? Do you guys have any suggestions other than masking tape in order to minimize re-work ?
What are your thoughts? Do let me know.