Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations SSS148 on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Fastener Finish Compatibility ?

Status
Not open for further replies.

Xanth64

New member
Nov 29, 2007
2
Question about compatibility of carbon fiber composite structure material and Ti Hi-Lite fasteners with Aluminum finish (Hi Kote 1).
 
Replies continue below

Recommended for you

What exactly is your question?

Wes C.
------------------------------
No trees were killed in the sending of this message, but a large number of electrons were terribly inconvenienced.
 
Well I was thinking that carbon and Aluminum basically make a battery so is there a finish coating for fasteners for use in composites structure.
Thanks for your help.
 
There are options. Contact your HiShear rep.

Cetyl Alcohol Lube

Anodize (Ti, Al)

or you can try a barrier layer



Wes C.
------------------------------
No trees were killed in the sending of this message, but a large number of electrons were terribly inconvenienced.
 
We usually use Al coated Ti or stainless fasteners when joining carbon to aluminum; they are always wet assembled with plenty of gunk (we usually put a layer of glass cloth between the carbon and the aluminum part, too). The coating is subject to attack if an electrical connection is made between the carbon and the coating, but it helps to avoid attack on the aluminum part, mostly from the fastener base material. For a major joint between carbon and aluminum we bush the fasteners in the Al.

Because the coating is subject to attack it should be avoided when joining carbon to non-aluminum parts. For carbon-carbon, carbon-Ti and carbon-st. st. (and st. st.-Ti, Ti-Ti, etc.) we usually use Ti, A-286 st. st. or Inco 718 fasteners bare.
 