Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations SSS148 on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Fatigue Equation for Cap Channel to Wide Flange Beam

Status
Not open for further replies.

alumpkin

Structural
Sep 11, 2000
69
Looking for guidance using Table A-3.1 in AISC manual for the fatigue equation for welding a cap channel to a wide flange beam. One option is continuous fillet welds and the other is intermittent fillet welds. It appears that for continuous fillet welds equation 3.1 is the correct one which has a stress limit of 16 ksi....but equation 3.4 for intermittent welds with a stress limit of 4.5 ksi....which seems really low.

Thanks for any insight.

Alan L. Lumpkin, MS, PE
Greenville, SC
 
Replies continue below

Recommended for you

"fatigue equation for welding a cap channel to a wide flange beam......"

I think intermittent welds get a hefty de=rate or even simply are forbitten whenever fatigue is involved.
Each of the start/stops is a significant stress concentration and potential weld defect site.
 