dlreed

Aerospace
Aug 13, 2001
5
I am looking for info and methodology on calculating fatigue life of a Inconel X750 wire torsion spring. Does anyone have some suggestions or references.
 
Replies continue below

Recommended for you

There is a great deal of design data for Inconel X-750 available from Special Metals, the producer of this alloy:


In general, for spring temper material (SAE AMS5699) at temperatures less than 260 C, the maximum stress should be kept below 690 MPa. This equates to ~ 45-55% of the ultimate tensile strength, depending on wire diameter. Some spring manufacturers use a more conservative 40% of UTS for the design stress.

Regarding methodology for analyzing fatigue life, I suggest investigating the Goodman method or a comparable fatigue life estimation method. The following link is an excellent paper that discusses the Goodman diagram:


Also, there are numerous handbooks and guidelines available, such as these:

Compression, Extension, Torsion and Garter Springs

Mechanical Springs by A.M.Wahl

Advanced Spring Design Software Version 6 (ASD6)

Spring Design Manual
 
Status
Not open for further replies.

Part and Inventory Search

Sponsor