Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations waross on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Filler material for Nickel plating

Status
Not open for further replies.

Drjones

Aerospace
Aug 20, 2008
5
I am working on a project that involves using electroless nickel plating on aluminum parts. Some of these parts have .1-.5 wide troughs, for instrumentation, that need to be filled and plated over for a uniform appearance. I am looking for a conductive, epoxy-like material that can fill these gaps smoothly and accept the nickel plating. I am trying to avoid the cost/lead time of plating the parts, soldering the gaps, than replating...

The only product I have found, so far, that seems applicable was called TRA-DUCT 2705 made by Tra-Con Inc. I can't find out much about it or where to by it though.

Hopefully this problem has come up before and someone here has some good ideas...
 
Replies continue below

Recommended for you

I guess I'm not using the right queries...were u able to find the answer easily with a search engine btrueblood?
 
Status
Not open for further replies.

Part and Inventory Search

Sponsor