Dear Gents,
I have a problem understanding Table QW-451.4 in ASME IX so i will go with direct questions hoping the answers will solve my confusion.
- According to table QW-451.4 If i have a WPS with a qualified range for groove welds from 3mm to 25 mm can i use this WPS to weld a fillet joint on a 30mm or 50mm Joints ?
- Also, If i have a WPS for a groove weld but this time with Preheat and PWHT Included shall i use the same PWHT and preheat requirement for welding a fillet weld if applicable ?
- I am in a situation now where i have a WPS for 3mm to 25 mm and i need to join two 35mm plates
together with fillet welds, can i do that according to tha table?
Thanks in advance
I have a problem understanding Table QW-451.4 in ASME IX so i will go with direct questions hoping the answers will solve my confusion.
- According to table QW-451.4 If i have a WPS with a qualified range for groove welds from 3mm to 25 mm can i use this WPS to weld a fillet joint on a 30mm or 50mm Joints ?
- Also, If i have a WPS for a groove weld but this time with Preheat and PWHT Included shall i use the same PWHT and preheat requirement for welding a fillet weld if applicable ?
- I am in a situation now where i have a WPS for 3mm to 25 mm and i need to join two 35mm plates
together with fillet welds, can i do that according to tha table?