phamENG
Structural
- Feb 6, 2015
- 7,626
Quick question - what are the limitations on a fillet weld to the side of the pipe? Particularly the diameter of the pipe. Welding a 3/8" plate to the side of an 8" round HSS probably isn't an issue, but what about to the side of a 3" pipe? The tighter radius creates a larger "angle" and the joint starts to look like a two-sided skewed fillet.
My thought is that it would be specified as a fillet but with the throat called out rather than the leg. For example, if I wanted a weld to develop the strength equivalent to a 90o fillet welded joint, I would put (0.178) in the weld symbol rather than 0.25 or 1/4. Sound about right?
My thought is that it would be specified as a fillet but with the throat called out rather than the leg. For example, if I wanted a weld to develop the strength equivalent to a 90o fillet welded joint, I would put (0.178) in the weld symbol rather than 0.25 or 1/4. Sound about right?