We have been tasked to close under ground storage tank in place. The tank was constructed but was never used. The tank top is made up with 1 ft concrete slab. The top of the concrete slab is 5 ft below the grade filled with soil. The tank is 130 ft long 35 ft wide and 25 ft deep (it's huge!)Void volume is close to 5000 cubic yard. One idea is to use cement/sand mixture which could flow. This is not done under any environmental law and we don't have to do any sampling.
Any comments on the idea of using cement/sand mixture? Any thoughts on how to implement it? What would be the cost of flowable fill per cubic yard?