Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations pierreick on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

FIRE DESIGN REQUIREMENT FOR WOOD MEMBERS

Status
Not open for further replies.

JKJohn

Structural
Oct 27, 2008
49
Hello -
I am using Woodworks sizer and concept. It seems that the software is requiring every design for all wood members to be verified for fire design.
Is this a requirement in the IBC? or is it just something WoodWorks folks decided to added?
Thanks
John
 
Replies continue below

Recommended for you

Fire design can impact the strength we assign to wood members. The only time I have encountered this is in the pre-qualified wall assemblies for fire resistance. There is an assembly using 2x studs, and in the footnote of the table a note that requires the strength of studs to be reduced by a %.
 
I haven't used sizer to IBC, but to my local codes, NBCC and CSA, fire design is an option we can turn on and off.
 
I actually noticed the same thing yesterday. It isn't doing it for everything - only joists. Pretty annoying, really. I can't find the toggle either, and I'm pretty sure it wasn't doing it Friday.
 