gafoorkti
Materials
- May 18, 2011
- 51
As per clien't specification, Wafer Butterfly valve (EPDM lined) shall be pressure to API 607. When we forwarded the same to our vendor, our vendor' clarification as follows:
"EPDM/Rubber lined Butterfly valve is not fire safe since it cannot be fire tested."
Instead they submitted "certificate of fire approval" from Lloyd Register which was not accepted by client. Client insisting for fire test as per API 607.
Any suggestion/advice would be much appreciated.
"EPDM/Rubber lined Butterfly valve is not fire safe since it cannot be fire tested."
Instead they submitted "certificate of fire approval" from Lloyd Register which was not accepted by client. Client insisting for fire test as per API 607.
Any suggestion/advice would be much appreciated.