Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations 3DDave on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

[FLANGE COSMETIC FULL RATE AND NORMAL ]

Status
Not open for further replies.

gguliye

Industrial
Apr 17, 2019
117
Dear Team,
I am currently working one of the projects and noticed unfamiliar terms such as cosmetic flange, full rate flange and normal flange. What are the differences between them>
regards,
 
Replies continue below

Recommended for you

Something new everyday.....
What's the industry for, or the process application?
 
Hi. "Cosmetic Flange" related to a PSV or Safety Relief Valve.
What it means is that the flange has the dimensions and profile and/or the ability to fit the designated flange rating but is NOT FULLY RATED to the designated pressure class.
Example: A 2" x H x 3" safety relief valve can have a 300# inlet flange fully rated and 150# standard outlet flange.
For whatever reason, the end user requires the outlet to be 300# maybe to mate up with existing pipework.
The manufacturer would then supply a non standard 2 x H x 3 300# x 300# COSMETIC OUTLET
This means that the manufacturer has taken his standard 300 x 150 body casting and machined the outlet to 300# dimensions - in many cases the outside diameter will be less than 300# but it does not matter since the pressure is restricted to 150# class (limited by API-526 or valve design). Some manufacturers have enough material on a raw body casting to actually maintain a 300# machined outlet. Most however will not and where requested, the manufacturer will get his body casting modified to allow full sized 300#. This option is not fully rated since the body (wall thickness) governs the outlet rating. In all of these examples, it can be said that the outlet flange is cosmetic only.

Per ISO, only the term Safety Valve is used regardless of application or design.
 