Nov 4, 2016 #1 AshaPatel Mechanical Mar 14, 2016 11 0 0 KR from where to check the flatness & Plating of octagonal ring gasket. If the gasket is as per ASME B16.20. Not find in the B16.20.
from where to check the flatness & Plating of octagonal ring gasket. If the gasket is as per ASME B16.20. Not find in the B16.20.
Nov 14, 2016 #2 jose0012000 Chemical May 21, 2015 9 0 0 US Flatness should be a customer or process requirement and the plating can be evaluated with a no or destructive technique analysis. Upvote 0 Downvote
Flatness should be a customer or process requirement and the plating can be evaluated with a no or destructive technique analysis.