A_WAHAB
Mechanical
- Apr 28, 2024
- 6
We have a floating roof tank which is used for storage of diesel. Following are the tank specification.
Diameter of Tank: 34 meter
Height of tank : 14 meters
Roof is double deck type
Make: Bernard & Smith
The roof of tank is double deck type and last refurbishment of tank was done in 2000 in which roof outer surface was cleaned and painted and inner surface was inspected.
Tank wall to floating roof seals were also replaced and currently no vapors leak is observed from tank wall to roof seal.
In recent rain event we have water level raised up inside the tank (measured and confirmed by DIP ) from 782 mm to 962 mm, which means around 200 tons of water went inside of tank. This was also confirmed as little water was found coming out of tank drain line. The roof water drain line also runs inside of tank to opening at bottom of tank.
We are planning to inspect the tank pontoons while in mean while can you guys help me in establishing following causes
1. From where the water went inside of tank either from Roof or drain line?
2. Whether there is chance of roof tilt or sink ?
3. What other precautions/inspection we have to perform?
Any feedback will help a lot
Diameter of Tank: 34 meter
Height of tank : 14 meters
Roof is double deck type
Make: Bernard & Smith
The roof of tank is double deck type and last refurbishment of tank was done in 2000 in which roof outer surface was cleaned and painted and inner surface was inspected.
Tank wall to floating roof seals were also replaced and currently no vapors leak is observed from tank wall to roof seal.
In recent rain event we have water level raised up inside the tank (measured and confirmed by DIP ) from 782 mm to 962 mm, which means around 200 tons of water went inside of tank. This was also confirmed as little water was found coming out of tank drain line. The roof water drain line also runs inside of tank to opening at bottom of tank.
We are planning to inspect the tank pontoons while in mean while can you guys help me in establishing following causes
1. From where the water went inside of tank either from Roof or drain line?
2. Whether there is chance of roof tilt or sink ?
3. What other precautions/inspection we have to perform?
Any feedback will help a lot