Jun 8, 2009 #1 brin Aerospace Mar 12, 2000 122 0 0 CA we have a drawing callout for 2024-T851 plate per FMS 1075. Does anyone recognize that spec (FMS 1075)?
we have a drawing callout for 2024-T851 plate per FMS 1075. Does anyone recognize that spec (FMS 1075)?
Jun 8, 2009 #2 rb1957 Aerospace Apr 15, 2005 15,595 0 36 CA F's Manufacturing Spec ? Fokker ? Fairchild ? Foeing ?? Upvote 0 Downvote
Jun 8, 2009 #3 IRstuff Aerospace Jun 3, 2002 44,355 4 38 US Ask the guy who supplied the drawing? TTFN FAQ731-376 Upvote 0 Downvote
Jun 15, 2009 #4 HANDCALC Aerospace Jun 28, 2004 35 0 0 CA Could these be Lockheed or General Dynamics drawings? Upvote 0 Downvote
Jun 30, 2009 #5 HPAlloys Materials Jun 30, 2009 3 0 0 US FMS in our company means it is a Fisher Material Specification. Are you working on a valve/control part? Upvote 0 Downvote
FMS in our company means it is a Fisher Material Specification. Are you working on a valve/control part?
Jul 8, 2009 1 #6 BrianKer Aerospace Jul 8, 2009 1 0 0 Hello Mr Brin....Yes that is a common GD spec used on vintage aircraft like the Corvair I believe. I might have it here somewhere if you want me to look, could take time I'm afraid. Upvote 0 Downvote
Hello Mr Brin....Yes that is a common GD spec used on vintage aircraft like the Corvair I believe. I might have it here somewhere if you want me to look, could take time I'm afraid.