This usage is applicable to Mil-STD-7885 blind rivets.
Requirement #3 is surprising, unless I accept that the locking ring is always effective, which I don't, having pulled a few Cherrys myself.
So often, the reason for using the blind rivet is that the tail is in an inaccessible area, hence uninspectable.
The tribal knowledge that has reached me forbids using these in critical locations. The comparison with #7 does not make this clearer.

MS33522C_Rivets_Blind_Structural_Design_Requirements_pfrmit.png


 
Replies continue below

Recommended for you

wow … "chemically expanded blind rivets" ??

another day in paradise, or is paradise one day closer ?
 
SW... FYI only...

MIL-R-7885/1 thru /238[?] [Cherry Max style] blind rivets have, for the most-part, been replaced/superseded by NAS9301 thru NAS9314.

Regards, Wil Taylor

o Trust - But Verify!
o We believe to be true what we prefer to be true. [Unknown]
o For those who believe, no proof is required; for those who cannot believe, no proof is possible. [variation,Stuart Chase]