Hi all,
I've been tasked with coming up with a company-wide standard checklist sheet for foundation inspections prior to pouring the concrete and was hoping to tap into the vast pool on knowledge available on this site. I have noted down an approximate outline of what I intend to cover.
Any further suggestions/examples would be greatly appreciated...
Inspection Specifics
-Site
-Date/Time
-Weather
-Inspector
-Contact on-site
-Site Risks
Source Information
-Drawings
-Specification
Inspected Elements
-Blinding layer
-Reinforcement spacing/diameter/cover/support chairs/splices/laps/....
-Shoring
-Waterproofing
-Holding Down Bolts
Observations
Verbal Instruction issued on site
I've been tasked with coming up with a company-wide standard checklist sheet for foundation inspections prior to pouring the concrete and was hoping to tap into the vast pool on knowledge available on this site. I have noted down an approximate outline of what I intend to cover.
Any further suggestions/examples would be greatly appreciated...
Inspection Specifics
-Site
-Date/Time
-Weather
-Inspector
-Contact on-site
-Site Risks
Source Information
-Drawings
-Specification
Inspected Elements
-Blinding layer
-Reinforcement spacing/diameter/cover/support chairs/splices/laps/....
-Shoring
-Waterproofing
-Holding Down Bolts
Observations
Verbal Instruction issued on site