I have a concrete foundation supporting concrete column.
Size of foundation is 3000 mm x 3000 mm x 600 mm thick.
There are bottom and top reinforcing for the foundation.
At the vertical face (perimeter) of the foundation, I would put vertical rebars 10M @300 mm spacing with horizontal hook at each end. Also I would put one horizontal 10M bars all around at mid-height.
Reason for this is to prevent concrete cracking/splitting.
Question: Are these extra reinforcing necessary? Is there any code related requirements for this?
Size of foundation is 3000 mm x 3000 mm x 600 mm thick.
There are bottom and top reinforcing for the foundation.
At the vertical face (perimeter) of the foundation, I would put vertical rebars 10M @300 mm spacing with horizontal hook at each end. Also I would put one horizontal 10M bars all around at mid-height.
Reason for this is to prevent concrete cracking/splitting.
Question: Are these extra reinforcing necessary? Is there any code related requirements for this?