I have a problem with a HDPE living hinge. When I bend the hinge it breaks.
It's a tiny hinge, only 0.005" thick and 0.030" wide. I have made it for years without a problem, but now the molders give me parts that crack and they can't seem to figure out why.
I am NOT a polymer engineer. I would appreciate any help.
It's a tiny hinge, only 0.005" thick and 0.030" wide. I have made it for years without a problem, but now the molders give me parts that crack and they can't seem to figure out why.
I am NOT a polymer engineer. I would appreciate any help.