Free fall of concrete - Concrete pour over a standing water in a caisson 3

Status
Not open for further replies.

ebooya

Civil/Environmental
Nov 23, 2020
2
Hello all,

Does anyone try pouring an anti-washout concrete (SCC)over a standing water in a caisson? Is this possible?

Also, the dewatering of the caisson is not possible or the rate of water intake is higher than the dewatering rate.

Looking for your thoughts and help.

Thanks.
 
Replies continue below

Recommended for you

You need to make your caisson less porous.

Or get bigger pumps.

More details needed.

Remember - More details = better answers
Also: If you get a response it's polite to respond to it.
 
agree with miningman, tremie the concrete in. Essentially this is a pipe that you start at the bottom of your caisson and pump the concrete in under the water. As the concrete fills the caisson hole, it will push the water up.
 
ebooya,

I agree with miningman & Jayrod12, use a tremmie to place the concrete below the water surface.

As you place the concrete raise the bottom of the tremmie pipe (maybe a canvas tube) as the concrete is placed. Always keep the bottom of the tremmie tube below the top of the new concrete so there is a seal.

Any contractor who wants to bid on the job should be familiar with the concept.

Jim

 
Thank you all for your feedback and your responses. I appreciate it.
 
Your are better off to dewater your cofferdams with submersible pumps before the concrete pours. The tremie pours we did were to seal up the bottom of the cofferdams before the concrete pours.
 

I've done fully submerged coffer dams by tremie method...

Rather than think climate change and the corona virus as science, think of it as the wrath of God. Feel any better?

-Dik
 