Friction coefficient between soil and polythene covered concrete 1

Status
Not open for further replies.

LTISGEO

Geotechnical
Oct 9, 2014
4
Hi Good Day everybody
Can anyone give me some guidance about Friction coefficient between soil and polythene covered concrete footing?
thanks
 
Replies continue below

Recommended for you

My experience is the value is near zero.

I once had a load of prepared sand on my trailer for ice removal purposes when I lived in the country. Since it was salty sand, I first put a sheet of plastic on trailer. In going home I went up a road at about 10 degrees slope. Then I turned onto a side road at no more than 20 degrees lope, probably 15. Getting home I was much amazed to see the trailer empty. Going back there was a neat pile of sand on the plastic in the middle of the road at the steeper slope. I suggest you do a similar test.
 
OG, very nice example. I also consider the value to be zero. For example, if we have a plastic moisture barrier sheet underneath the floor slab, I recommended no consider contribution of lateral resistant from the slab friction with the soils.
 
To which I'll ask, what's the end game? I mean If I was some researcher and claimed to know the answer was 8 degrees, what would you then do with the number?

f-d

ípapß gordo ainÆt no madre flaca!
 
Thnaks every body. the real scenaio was to conclude the fondation recommnedation.
 