Galvanising - Baling (Xpost)

Status
Not open for further replies.

bangerjoe

Industrial
Oct 16, 2013
35
Previously submitted in other forum for corrosion.

Hi Guys,

i have a drawing with galvanising specifications as the general notes.

one note is "Baling" is not permitted. (it even has the " symbol, as if it is a colloquialism).

Does anyone know what Baling is and why it would be prohibited?
 
Replies continue below

Recommended for you

I don't know for sure, but might it mean that you can't wire or strap together a group of pieces and put them into the hot zinc.
 
I've never heard the term used, but that's how I would interpret it as well.
 
What Jed said or maybe check the Urban Dictionary
 
It is apparently related to bale, as will be clear from this Link.