Taro
Structural
- Nov 29, 2000
- 713
Any comments on the pros and cons of hot-dipped vs. mechanically galvanized bolts? The application is statically loaded A325 bolts in a sewage pump station. The bolts will be subjected to constant high humidity and possibly intermittent water contact.