Hi everybody,
I have to purchase some pressure vessels and some filters which shall contain well water.
The process specification says that the Vessel can be designed and manufactured taking into account as main material Carbon Steel plus 3mm of corrosion allowance plus glass flake as internal lining. Moreover all internals (vortex breaker, internal baffle,etc...) shall be made by super duplex or plastic material.
Does anyboby have experience with this type of internal lining applications?
Are there some precautions or limitations in applaying this type of lining in some cases like us high pressure apllications, small diameter vessel, etc..?
Furthermore for small diameter housing filters (500mm) could be better to make the internal lining in Super Duplex Material, considering the internal lining glass flake costs and application?
Which kind of NDE can be performed on these lined Vessels?
Any clarification on the matter would be greatly appreciated.
I have to purchase some pressure vessels and some filters which shall contain well water.
The process specification says that the Vessel can be designed and manufactured taking into account as main material Carbon Steel plus 3mm of corrosion allowance plus glass flake as internal lining. Moreover all internals (vortex breaker, internal baffle,etc...) shall be made by super duplex or plastic material.
Does anyboby have experience with this type of internal lining applications?
Are there some precautions or limitations in applaying this type of lining in some cases like us high pressure apllications, small diameter vessel, etc..?
Furthermore for small diameter housing filters (500mm) could be better to make the internal lining in Super Duplex Material, considering the internal lining glass flake costs and application?
Which kind of NDE can be performed on these lined Vessels?
Any clarification on the matter would be greatly appreciated.