Hi guys, was hoping someone could help me out with this question. I am wanting to bond a polyurethane textile (40oz/yd2) to FRP. The manufacturer has recommended a few different glues, one being a 3532 3m urethane adhesive, and another being an epoxy adhesive, and then an acrylic adhesive as well. The application is marine so it would be exposed to all those associated elements. What else would I want to take into account when choosing an adhesive to bond these? Would one be a better option than the other?
 