Dears,
Is it possible to create "golden weld" for internal coating pipeline after hydrostatic testing, and what's the technique used for coating "golden weld" ?
note: we have main pipeline 20" and two branches 12" , where each pipeline will be hydrostatic tested separately and then two branches will be connected the main pipeline after hydrostatic test "golden weld"
thanks in advance![[smile] [smile] [smile]](/data/assets/smilies/smile.gif)
Is it possible to create "golden weld" for internal coating pipeline after hydrostatic testing, and what's the technique used for coating "golden weld" ?
note: we have main pipeline 20" and two branches 12" , where each pipeline will be hydrostatic tested separately and then two branches will be connected the main pipeline after hydrostatic test "golden weld"
thanks in advance