Ineedto5s
Mechanical
- Oct 15, 2018
- 18
I have an issue with carrier rings for a large lap table. They require a 45 degree chamfer in order to push the slurry on the table. Problem is that it's approximately a 16.5 inch alumina ring, and we do not have an grinder with a big enough chuck. We do however have a CNC lathe (with turret) with a big enough chuck. Any options to make this work?