Hi all,

I need some advise on the following issue.
My customer just rejected some 150# low pressure screw fitting due to some grinding mark on the surface.

Is there any standard stating that slight grinding mark is allow. I browse through ASTM A351, but could not found anything related to
grinding/surface finishing.

Anyone can help?
Thanks in advance.
 
Replies continue below

Recommended for you

ASTM A802 should tell you what you need to know. Also, the customer drawings may give you the finish requirements.
 
thanks for the advise bro jwhit
 